Investigative Process Uncovers Cause of Surface Tearing In Cold Box Aluminum Alloy Pipe Components | AIChE

Investigative Process Uncovers Cause of Surface Tearing In Cold Box Aluminum Alloy Pipe Components

Type

Conference Presentation

Conference Type

AIChE Spring Meeting and Global Congress on Process Safety

Presentation Date

March 14, 2011

Duration

30 minutes

Skill Level

Intermediate

PDHs

0.50

Abstract: This paper describes the investigative tools and techniques, learning’s, and logistical challenges faced by an international team assembled to uncover the source of surface tears in newly manufactured 6061 aluminum alloy pipe elbows. The cold box, with its complex piping layout, and a tight project construction schedule required a thoughtful and effective strategy for non-destructive testing (NDT), component review and sampling, and mechanical- and metallurgical testing of similarly-manufactured replicate pipe elbows. Good cooperation between the end user operator, engineering, procurement & construction (EPC) company, subject matter experts, and cold box and pipe elbow manufacturer culminated in a successful outcome and repair.

Presenter(s) 

Once the content has been viewed and you have attested to it, you will be able to download and print a certificate for PDH credits. If you have already viewed this content, please click here to login.

Language 

Checkout

Checkout

Do you already own this?

Pricing

Individuals

AIChE Member Credits 0.5
AIChE Pro Members $15.00
AIChE Graduate Student Members Free
AIChE Undergraduate Student Members Free
AIChE Explorer Members $25.00
Non-Members $25.00